Quantum Composites Lytex® 9063 63% Glass Fiber Epoxy SMC

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Composite SMC , Epoxy , Filled/Reinforced Thermoset
Manufacturer Quantum Composites
Trade Name Lytex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites Lytex® 9063 63% Glass Fiber Epoxy SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lytex 9063 is a high performance, glass fiber reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance and excellent electrical properties. It meets the requirements of MIL-M-46069 and MIL-M-46892. Form and Color = Sheet, Black. Glass Length (Std.) = 0.5"Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
ASTM D792
Water Absorption 0.080 %
0.080 %
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 241 MPa
35000 psi
ASTM D638
Flexural Yield Strength 455 MPa
66000 psi
ASTM D790
Flexural Modulus 18.0 GPa
2610 ksi
ASTM D790
Izod Impact, Notched 18.7 J/cm
35.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 300 °C
>= 572 °F
Deflection Temp; Load not reported; ASTM D648
Shrinkage 0.0010 %
0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 3.00e+14 ohm-cm
3.00e+14 ohm-cm
ASTM D257
Dielectric Constant 4.3

@Frequency 100 Hz
4.3

@Frequency 100 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
ASTM D149
Dissipation Factor 0.0070

@Frequency 100 Hz
0.0070

@Frequency 100 Hz
ASTM D150
Processing Properties Metric English Comments
Processing Temperature 121 - 163 °C
250 - 325 °F
Mold temperature