Qualchem Danamid AFGFS2HUV14 Polyamide 66, 14% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid AFGFS2HUV14 Polyamide 66, 14% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reinforced with glass fiber. Impact modified, heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial lights.Information provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
DIN 53479
Filler Content 12 - 16 %
12 - 16 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 70.0 MPa
>= 10200 psi
50 mm/min; ISO 527-1,2
Charpy Impact Unnotched >= 1.50 J/cm²

@Temperature 23.0 °C
>= 7.14 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched >= 0.500 J/cm²

@Temperature 23.0 °C
>= 2.38 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
DIN 53461
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Comparative Tracking Index 550 V
550 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 2.0 - 2.2 %
2.0 - 2.2 %
DIN 53714