Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Qualchem Danamid AFGFLPX0-35 Polyamide 66, 35% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid AFGFLPX0-35 Polyamide 66, 35% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reinforced with glass fiber, red phosphorous flame retardant, V-0Information provided by Qualchem Zrt.
Physical Properties Metric English Comments
Filler Content 33 - 37 %
33 - 37 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 90.0 MPa
>= 13100 psi
50 mm/min; ISO 527-1,2
Charpy Impact Unnotched >= 2.00 J/cm²

@Temperature 23.0 °C
>= 9.52 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
MSZ 10383
Glow Wire Test 960 °C

@Thickness 3.50 mm
1760 °F

@Thickness 0.138 in
IEC 685-2-1
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
DIN 53482
Comparative Tracking Index 600 V
600 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 1.8 - 2.0 %
1.8 - 2.0 %
DIN 53714
Users viewing this material also viewed the following: