Reinforced with glass fiberInformation provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
DIN 53479
Filler Content 18 - 22 %
18 - 22 %
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 140 MPa
<= 20300 psi
50 mm/min; ISO 527-1,2
Elongation at Break 4.0 %
4.0 %
ISO 527-1,2
Charpy Impact Unnotched <= 3.00 J/cm²

@Temperature 23.0 °C
<= 14.3 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched <= 1.00 J/cm²

@Temperature -20.0 °C
<= 4.76 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
<= 1.00 J/cm²

@Temperature 23.0 °C
<= 4.76 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
DIN 53461
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Comparative Tracking Index 375 V
375 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 1.5 - 1.8 %
1.5 - 1.8 %
DIN 53714