Qualchem Danamid AFEHUV Polyamide 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid AFEHUV Polyamide 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat and UV stabilized, for long-lasting use at 120-130°C, protected against artificial lightInformation provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 80.0 MPa
>= 11600 psi
50 mm/min; ISO 527-1,2
Tensile Modulus >= 2.50 GPa
>= 363 ksi
ISO 527-1,2
Charpy Impact Unnotched NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
DIN 53453
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched 0.300 J/cm²

@Temperature -20.0 °C
1.43 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
DIN 53461
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Processing Properties Metric English Comments
Moisture Content 1.2 - 1.5 %
1.2 - 1.5 %
DIN 53714
Descriptive Properties Value Comments
Heat Stability (24h 90°C) No visible change
Users viewing this material also viewed the following: