Quadrant EPP Symalit® 1000 ETFE unfilled, lining industries (ISO Data)

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE/ECTFE, Molded/Extruded
Manufacturer Quadrant Engineering Plastics Products
Trade Name Symalit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Symalit® 1000 ETFE unfilled, lining industries (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Service temperature range from -190 °C up to +155 °C / -310 °F up to +311 °F Mechanical and technical features correspond to those of ECTFE Excellent weather proof and radiation proof Low water adsorption Excellent resistance of abrasion
Compliance Properties Metric English Comments
3A-Dairy No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable