Pyrotek TS-102 Thermoset Electrical Insulation Product (Nema Grade: X)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek TS-102 Thermoset Electrical Insulation Product (Nema Grade: X).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper reinforcement, Phenolic Resin, Natural Color. High mechanical strength. Electrical properties are secondary.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasketsAdvantagesHigh insulation properties High strength Low moisture absorption High temperature resistance Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.362 g/cc
0.04921 lb/in³
Water Absorption 2.0 %
2.0 %
Mechanical Properties Metric English Comments
Flexural Strength 207 MPa
30000 psi
Compressive Strength 262 MPa
38000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 138 °C
280 °F
Continuous
Electrical Properties Metric English Comments
Dielectric Strength 18.0 kV/mm
457 kV/in