Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Stainless Steel Mesh Core

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Stainless Steel Mesh Core.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stainless steel mesh. Flat.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 870 °C
1600 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved