Pyrotek Silicone Rubber Core

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Silicone Rubber Core.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone rubber. Custom-shaped profiles.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrotek.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F