Pyrotek Pyroboard™ S1200 Roller

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name Pyroboard™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyroboard™ S1200 Roller.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyroboard™ S1200 is a long wearing durable, soft covering. It must be used in high heat areas in order for it to realize its full effectiveness. The heat helps to sinter the materials so that the roll surface becomes harder as it is used. This material can be used in both preheat and annealing sections of a furnace. S1200 has shown the ability to be used in all types of furnaces that require the roll to be enclosed or in an open application.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1200 °C
2190 °F