Category Ceramic , Carbide
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pinnacle Thermocouple Protection Tubes O'-Sialon (Bonded Silicon Carbide) TCPT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The robust properties of Pinnacle Thermocouple Protection Tubes make it a superior alternative to competitive tubes in temperature measurement, maintenance and product life areas.ApplicationsCrucible furnaces Degassing crucibles Holding furnaces Casting areas AdvantagesNon-wetting to aluminum and its alloys Less dross build up at metal line Superior response time Narrow temperature control band for energy conservation Excellent thermal shock resistance Longer life Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.60 g/cc
0.0939 lb/in³
Open Porosity 18.1 %
18.1 %
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0780 GPa
11.3 ksi
Modulus of Rupture 0.0340 GPa
4.93 ksi
Thermal Properties Metric English Comments
CTE, linear 4.40 µm/m-°C

@Temperature 20.0 °C
2.44 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 8.97 W/m-K

@Temperature 720 °C
62.3 BTU-in/hr-ft²-°F

@Temperature 1330 °F
9.05 W/m-K

@Temperature 540 °C
62.8 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10.21 W/m-K

@Temperature 300 °C
70.86 BTU-in/hr-ft²-°F

@Temperature 572 °F