Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Fiberseal Paper C-6 Ceramic fiber paper

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name Fiberseal Paper
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Fiberseal Paper C-6 Ceramic fiber paper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C-6 is an economical, high strength, Fiberseal paper composed of ceramic fibers, inert fillers and fiberglass.ApplicationsGaskets Seals Linings AdvantagesLow shrinkage Good dielectric properties Uniform thermal conductivity Easily shaped Low-cost Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.210 g/cc
0.00759 lb/in³
Binder 0.060 - 0.16
0.060 - 0.16
organic
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 705 °C
1300 °F
Electrical Properties Metric English Comments
Dielectric Strength 2.482 kV/mm
63.04 kV/in
Users viewing this material also viewed the following: