Pyrotek Dry Ground Bone Ash Coating for non-ferrous metals

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Dry Ground Bone Ash Coating for non-ferrous metals.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemically inert, Dry Ground Bone Ash from Pyrotek is less dense than aluminum and will not effect the quality of castings. Bone Ash is a dry white coating which out performs red mud as a parting agent and adheres and packs well into troughs and launders. Its superior protection from skull build-up increases the life of trough sections, refractories and tools.ApplicationsSealant for refractory cracks Dry coating for refractory parts and tools Glass manufacturing Parting agent AdvantagesChemically inert Effectively releases skull Easy to apply Packs well into cracks Adheres to tools and refractories Information provided by Pyrotek.
Physical Properties Metric English Comments
Loss On Ignition <= 2.00 %

@Temperature 1200 °C
<= 2.00 %

@Temperature 2190 °F
Component Elements Properties Metric English Comments
Al2O3 0.21 %
0.21 %
CaO 53.2 %
53.2 %
Fe2O3 0.20 %
0.20 %
MgO 1.22 %
1.22 %
Na2O 1.36 %
1.36 %
Other 3.12 %
3.12 %
P2O5 40.1 %
40.1 %
SiO2 0.59 %
0.59 %
Descriptive Properties Value Comments
Wet Sieve Analysis Max 1%
Residue on +300 mesh, B.S. 410/1986