Process Technologies Inc Viton®/FKM Sanitary Gasket

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Process Technologies Inc
Trade Name Viton®/FKM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Process Technologies Inc Viton®/FKM Sanitary Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FKM is USP Class VI, FDA and 3A compliant. This material provides high acid and temperature resistance. It does not have strong Base resistance and performs very poorly when used with Ketones. FKM is not recommended for continuous use in SIPInformation provided by Process Technologies Inc
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204.44 °C
399.99 °F
Minimum Service Temperature, Air -28.89 °C
-20.00 °F
Descriptive Properties Value Comments
Compatibility for Chemicals Acetone
Good
Ammonia
Not Recommended
Hydrochloric Acid
Excellent
Hydrofluoric Acid
Limited
Hydrogen Peroxide
Excellent
Isopropyl Alcohol
Excellent
Nitric Acid
Excellent
Phosphoric Acid
Excellent
Sodium Hydroxide
Excellent
Sodium Hypochlorite
Excellent
Steam to 400ºF (204ºC)
Limited
Sulfuric Acid
Excellent