Material Notes:
Halogen-free PRETECH engineering thermoplastics enable environmentally friendly and cost efficient V-0 product solutions with excellent mechanical and electrical properties. PRETECH combines high thermal resistance with exquisite dielectric properties. This makes it optimal choice e.g. for demanding under the hood applications.Halogen-Free Eco-Friendly answer for industry’s needs:Environmental awareness and standards are guiding electronics industry towards green product solutions. With PRETECH the strict material requirements set by legislation and directives can be complied. PRETECH contains a unique combination of properties; high temperature resistance and exceptionally good mechanical properties. Excellent impact strength enables engineering of robust devices. The density of the material is very low and the advantage can be turned into lighter electronical devices.PRETECH for cables & electronics:Halogen free flame retardant UL 94-V0Very high HDT 185 °CVery high impact strengthExcellent dielectric strengthLow densityUnreinforced materialLow water absorptionCTI 200 VRoHS compliantInformation from Premix OY
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength 45.0 MPa
6530 psi
ISO 527
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Flexural Modulus 2.20 GPa
319 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Thickness 4.00 mm,
Temperature -20.0 °C
4.76 ft-lb/in²

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
25.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
11.9 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched (ISO) NB

@Thickness 4.00 mm,
Temperature 23.0 °C
NB

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
NB

@Thickness 4.00 mm,
Temperature -20.0 °C
NB

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 185 °C
365 °F
75/Method Bf
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
75/Method Af
Glass Transition Temp, Tg 200 °C
392 °F
ISO 11357
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 2.55
2.55
Dissipation Factor 0.00070
0.00070
Comparative Tracking Index 200 V
200 V
ISO IEC60112