Premix Thermoplastics PRESEAL 5020 Ni-Coated Graphite

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Premix Thermoplastics Inc.
Trade Name PRESEAL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PRESEAL 5020 Ni-Coated Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Highly conductive PRESEAL® thermoplastic elastomer compounds are injection-mouldable and extrudable plastics for EMI-gasket and -housing applications, among other uses. The material is an ideal choice for mass production applications since it enables fast cycle times and requires no aftercuring.Significant Cost-Savings Through Simplified Logistics Chain:A contract manufacturing company for electronics wanted to cut down the process steps and speed up the logistic process. The EMI shielding part of the process had to be outsourced, since the company was not able to process silicone rubber. That wasted both money and time. By changing the silicone rubber into PRESEAL® elastomer the company was able to carry out the moulding in-house and accelerate the logistic process significantly, not to mention the savings achieved in overall costs.Advantages in Design and Processing:Processing by normal thermoplastic processing methods; injection molding and extrusion. Easy processability enables product designs with complex shapes and sizes. Mass-production friendly; fast cycle times, no need for vulcanisation nor primers. Recyclable and RoHS compliant.Electrical and Mechanical PropertiesVolume resistivity from 0.003 to 0.03OcmAttenuation from 90 to 100dBLow compression setLow hardness in highly filled compoundLow melt viscosityInformation from Premix OY
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Compression Set 20 %

@Temperature 85.0 °C,
Time 86400 sec
20 %

@Temperature 185 °F,
Time 24.0 hour
Electrical Properties Metric English Comments
Volume Resistivity 0.030 ohm-cm
0.030 ohm-cm
Shielding Effectiveness 90 dB
90 dB
Copyright © lookpolymers.com All Rights Reserved