Premix Thermoplastics PREBLACK PE 799

Category Polymer , Thermoplastic
Manufacturer Premix Thermoplastics Inc.
Trade Name PREBLACK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PREBLACK PE 799.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PREBLACK PE 799 black masterbatch has been developed for the coloring of polyethylene films down to 40 microns. PREBLACK PE 799 can also be used for extruded and injection molded products made of polyethylene. PREBLACK PE 799 is an economical alternative when recycled films are produced. The added rubber in PREBLACK PE 799 enhances the film strength properties.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
When Produced
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Carrier PE-LD
Dosing, % 0.5 to 5
Depending on desired opacity
Light Fastness 8-Very Good
Pigmentation, % 40
General purpose carbon black (SRF-type)