PREBLACK PE 704-40 black masterbatch has been developed for the coloring of PE-LD, PE-LLD and PE-HD films when maximum UV-resistance and pureness is required.The moisture absorption of PREBLACK PE 704-40 is extremely low. The sulphur content in the carbon black is very low, too, preventing odor problems. PREBLACK PE 704-40 is also recommended for agricultural film applications. PREBLACK PE 704-40 does not contain silica, calcium carbonate or any other fillers.According to BgVV regulations PREBLACK PE 704-40 is approved for use in contact with foodstuffs as long as the content of carbon black less than 2.5% in the product produced.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
When Produced
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Carrier PE-LD
Dosing, % 0.5 to 10
Depending on desired blackness and UV-protection
Light Fastness 8-Very Good
Pigmentation, % 40
Special carbon black (p-type)