Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Thermoplastics PRE-ELEC® PE 1270  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PRE-ELEC® PE 1270  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 1270 has excellent mechanical properties and is easy to injection mould. Typical applications include injection molded technical parts where good impact strength in low temperatures is needed. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Linear Mold Shrinkage 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ISO 294-4
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
2.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.0 MPa
1600 psi
ISO 527
Elongation at Break 520 %
520 %
ISO 527
Modulus of Elasticity 0.220 GPa
31.9 ksi
ISO 178
Izod Impact, Notched NB

@Thickness 4.00 mm,
Temperature -20.0 °C
NB

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
NB

@Thickness 4.00 mm,
Temperature 23.0 °C
NB

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched NB

@Thickness 4.00 mm,
Temperature -20.0 °C
NB

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
NB

@Thickness 4.00 mm,
Temperature 23.0 °C
NB

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
Rate A; ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
ISO D-257
Surface Resistance <= 1e+05
<= 1e+05
ISO D-257
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Drying Temperature 90.0 °C

@Time 10800 sec
194 °F

@Time 3.00 hour
If stored for longer than 1 year
Moisture Content <= 0.15 %
<= 0.15 %
When Produced
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Color Black
Injection Speed Moderate
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved