Material Notes:
PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE-ELEC ESD 12-000 are washable, reusable and recyclable. Surface resistance values of 108 ohms (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved with optimum processing parameters.PRE-ELEC ESD 12-000 can be colored into various bright colors. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break 35 %
35 %
ISO 527
Tensile Modulus 1.38 GPa
200 ksi
ISO 527
Izod Impact, Notched 1.60 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched NB

@Thickness 4.00 mm,
Temperature 23.0 °C
NB

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75/Method Af
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+8 ohm-cm
<= 1.00e+8 ohm-cm
ISO D-257
Surface Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ISO D-257
Static Decay <= 2.0 sec
<= 2.0 sec
ISO IEC 61340-5-1
Processing Properties Metric English Comments
Melt Temperature 185 - 210 °C
365 - 410 °F
Mold Temperature 80.0 - 105 °C
176 - 221 °F
Drying Temperature 80.0 °C

@Time 10800 - 14400 sec
176 °F

@Time 3.00 - 4.00 hour
Pre-drying in a dehumidifier
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Descriptive Properties Value Comments
Injection Speed Moderate