Precision Polymer Engineering V90W Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V90W Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Off-White Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600. ASTM designation = FKM. ISO designation = FPM.Applications: Formulated for use in equipment associated with the production of foodstuffs intended for human consumption.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
°IRHD; ASTM D1415
100
100
°IRHD, +10 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 7.50 MPa
1090 psi
-25% change after 72 hours @ 250°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 75 %
75 %
-25% change after 72 hours @ 250°C; ASTM D412
100 %
100 %
ASTM D412
Compression Set 50 %
50 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F