Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V90H Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V90H Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA). ASTM designation = FKM. ISO designation = FPM.Applications: Excellent oil and heat resistance. Ideal for mouldings which are required to operate within the approximate temperature range of -20° to +200°C, in contact with air.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
°IRHD; ASTM D1415
84 - 96
84 - 96
°IRHD, ±6 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 8.80 MPa
1280 psi
-20% change after 72 hours @ 250°C; ASTM D412
11.0 MPa
1600 psi
ASTM D412
Elongation at Break 80 %
80 %
-20% change after 72 hours @ 250°C; ASTM D412
100 %
100 %
ASTM D412
Compression Set 20 %
20 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Users viewing this material also viewed the following: