Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V60D Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V60D Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet Aerospace Specifications DTD5612A and DTD5543B Grade 60.Applications: Mouldings which are required to operate within the approximate temperature range of -20° to +225°C, in contact with air, petroleum, silicone and diester-based liquids. The material is not suitable for use in contact with certain phosphate-ester-based liquids.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
60
60
°IRHD, 0 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 15.865 MPa
2301.0 psi
-5% change after 72 hours @ 250°C; ASTM D412
16.7 MPa
2420 psi
ASTM D412
Elongation at Break 260 %
260 %
ASTM D412
265.2 %
265.2 %
2% change after 72 hours @ 250°C; ASTM D412
Compression Set 5.0 %
5.0 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 225 °C
437 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Copyright © lookpolymers.com All Rights Reserved