Material Notes:
Golden Yellow, Silicone 55-65 °IRHD. Diesel liner ring grade. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and low temperature flexibility combined with low compression set performance. Used primarily for diesel cylinder liner O-Rings (coolant sealing).
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
66
66
°IRHD, +6 change after 672 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 7.50 MPa
1090 psi
ASTM D412
Elongation at Break 325 %
325 %
ASTM D412
Compression Set 14.2 %
14.2 %
70 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-60.0 °C
-76.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F