Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Perlast® G75S Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name Perlast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Perlast® G75S Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Perlast® G75S has been specifically developed to cope with a wide range of process media, potent active pharmaceutical ingredients (APIs) and aggressive cleaning agents, being especially suited to withstand steam-in-place (SIP) and clean-in-place (CIP) procedures within pipe work and vessels. G75S is also suitable for other critical applications such as Water-For-Injection (WFI) systems. Perlast® G75S is an all round material that can be used for all types of applications requiring FDA and USP Class VI compliance. It is suitable for use in all product contact applications including dry, aqueous and fatty media. Unlike other FDA compliant elastomers, Perlast® G75S is thermally stable at higher temperatures, and is ideal for use in applications which require exposure to temperatures up to 310°C (590°F) making it suitable for use in Stage II Sterilization processes. Perlast® G75S is suitable for both dynamic and static applications and can be moulded into O-rings and custom shapes.Applications: Recommended for use in pharmaceutical, bio-analytical and food processing applications, where both mechanical and chemical properties are crucial, and hygienic sealing capability is critical. Dynamic Seals: Split butterfly valve seals; Ball segment valve seals. Static Seals: O-rings; Pressure safety rings; Gaskets; Hygienic & sanitary couplings; Mechanical seals for stirring/mixing screws & pumps
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D1415
80
80
ASTM D2240
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D412
Elongation at Break 237 %
237 %
ASTM D412
100% Modulus 0.00880 GPa
1.28 ksi
ASTM D412
Compression Set 20 %
20 %
72 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
CTE, linear 300 µm/m-°C

@Temperature 20.0 °C
167 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 310 °C
590 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F