Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Perlast® G67P Translucent Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name Perlast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Perlast® G67P Translucent Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A translucent beige compound with semi-crystalline perfluoropolymer nano-filler, specially developed to meet the demands of the semiconductor and bio-analytical industries. Compatible with fluorine based chemistries and universally suitable for both wet and dry semiconductor processes including Lithography, Plasma, PVD, CVD, Etch, Stripping and Cleaning. Perlast® G67P combines a fully fluorinated polymer backbone, a fully fluorinated nano-filler system (no inorganic fillers) and a highly fluorinated cross-linking process, which results in a perfluoroelastomer with unrivalled purity and chemical resistance. Perlast® G67P has a significantly lower compressive modulus than traditional perfluoroelastomers, making it highly compliant. So for a given compression, it exhibits a low reaction force, this results in lower stress on the seal, which leads to longer life expectancy.Applications: Dynamic seals: gate valves; door seals; pendulum valves; ISO valves; bonded gates and lip seals. Static seals: O-rings; body seals; chamber lid seals; cathode assembly seals; electro-static-chuck seals; flange fittings. Wafer-handling products: end effector pads; vacuum suction pads. Wet and dry semiconductor processes: lithography; plasma; PVD; CVD; etch; stripping; cleaning. Laser/optical equipment.
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
ASTM D2240
60 - 70
60 - 70
°IRHD; ASTM D1415
Tensile Strength, Yield 18.3 MPa
2650 psi
ASTM D412
Elongation at Break 331 %
331 %
ASTM D412
100% Modulus 0.00345 GPa
0.500 ksi
ASTM D412
Compression Set 34.5 %
34.5 %
24 hours @ 200°C; ASTM D395
41 %
41 %
70 hours @ 204°C; ASTM D395
Thermal Properties Metric English Comments
CTE, linear 520 µm/m-°C

@Temperature 20.0 °C
289 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 275 °C
527 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Descriptive Properties Value Comments
Color translucent beige