Precision Polymer Engineering N80C Nitrile Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering N80C Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Nitrile Rubber, 75-85 °IRHD. High acrylonitrile (ACN) content (38%). Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. British Gas Specification BGC/PS/LC6 Class E, approval ref.: 71/6.11.iv. MSL lab code 2.R. Also meets British Standard BS2494 Type G.Applications: Elastomeric seals for use in pipelines carrying manufactured or natural gas at operating temperatures of -5° to +40°C and pressures up to 7 bar.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
85
85
°IRHD, +5 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 8.10 MPa
1170 psi
-10% change after 70 hours @ 100°C; ASTM D412
9.00 MPa
1310 psi
ASTM D412
Elongation at Break 112.5 %
112.5 %
-25% change after 70 hours @ 100°C; ASTM D412
150 %
150 %
ASTM D412
Compression Set 12 %
12 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Flash Point >= 300 °C
>= 572 °F