Precision Polymer Engineering F50A Fluorosilicone Rubber

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering F50A Fluorosilicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blue Fluorosilicone, 45-55 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexibility. Suitable for sealing petroleum oils and hydrocarbon fuels. Fluorosilicones are widely used in aircraft fuel systems.
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
°IRHD; ASTM D1415
Tensile Strength, Yield 7.50 MPa
1090 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
Compression Set 10 %
10 %
22 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-55.0 °C
-67.0 °F
ASTM D2137, Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F