Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering E90Q Ethylene Propylene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering E90Q Ethylene Propylene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Peroxide cured, Ethylene Propylene Terpolymer, 85-95 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600. To meet ASTM D2000/SAE J200 line call-out M8CA910, A25, B35, C32, EA14, F17.Applications: Excellent water and steam resistance with good compression set properties. Heat and chemical resistance is superior to that of sulphur cured EPDM.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
°IRHD; ASTM D1415
100
100
°IRHD, +10 change after 70 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 8.00 MPa
1160 psi
-20% change after 70 hours @ 125°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 60.0 %
60.0 %
-40% change after 70 hours @ 125°C; ASTM D412
100 %
100 %
ASTM D412
Compression Set 50 %
50 %
22 hours @ 125°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F