Material Notes:
Peroxide cured, Ethylene Propylene Rubber, 65-75 °IRHD. Copolymer of ethylene and propylene.Applications: Excellent water and steam resistance with good compression set properties. Superior heat and chemical resistance compared to sulphur cured EPDM. Not oil resistant.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
80
80
°IRHD, +10 change after 70 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 8.00 MPa
1160 psi
-20% change after 70 hours @ 125°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 120 %
120 %
-40% change after 70 hours @ 125°C; ASTM D412
200 %
200 %
ASTM D412
Compression Set 10 %
10 %
22 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F