Material Notes:
Sulphur cured, off-white Ethylene Propylene Terpolymer, 55-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title (CFR21), Section 177.2600. Extraction tested in distilled water.Applications: Suitable for repeated use with dry and aqueous foodstuffs intended for human consumption. Not suitable for use with fatty foodstuffs.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
75
75
°IRHD, +15 change after 168 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 11.04 MPa
1601 psi
-20% change after 168 hours @ 125°C; ASTM D412
13.8 MPa
2000 psi
ASTM D412
Elongation at Break 200 %
200 %
-20% change after 168 hours @ 125°C; ASTM D412
250 %
250 %
ASTM D412
Compression Set 64 %
64 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Non-brittle after 3 minutes
-40.0 °C
-40.0 °F
Flash Point >= 200 °C
>= 392 °F
Descriptive Properties Value Comments
Extraction Test, 21 CFR 177.2600 pass
Distilled Water