Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering C70H Chloroprene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering C70H Chloroprene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Off-white, Chloroprene Rubber, 65-75 °IRHD. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21) Section 177.2600.Applications: A versatile rubber with good compression set properties.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
85
85
°IRHD, +15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield >= 8.50 MPa
>= 1230 psi
-15% change after 70 hours @ 100°C; ASTM D412
>= 10.0 MPa
>= 1450 psi
ASTM D412
Elongation at Break 150 %
150 %
-40% change after 70 hours @ 100°C; ASTM D412
250 %
250 %
ASTM D412
Compression Set 50 %
50 %
22 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Non-brittle after 3 minutes
-40.0 °C
-40.0 °F
Flash Point >= 260 °C
>= 500 °F
Users viewing this material also viewed the following: