Potters Industries Spheriglass® Spacer Bead Solid Soda-Lime Glass Spheres

Category Ceramic , Glass , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Potters Industries
Trade Name Spheriglass®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries Spheriglass® Spacer Bead Solid Soda-Lime Glass Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These beads are specifically designed for controlling bond line thickness in adhesive bonding. These beads are manufactured and certified to meet the specification requirements of Raytheon HMS20-1776 and Boeing SCGMS-53004Information provided by Potters Industries.
Physical Properties Metric English Comments
Specific Gravity 2.30 - 2.70 g/cc
2.30 - 2.70 g/cc
Optical Properties Metric English Comments
Refractive Index 1.50 - 1.55
1.50 - 1.55
Component Elements Properties Metric English Comments
Free Iron <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Color colorless
Shape spherical