Potters Industries Conduct-O-Fil® SC04P10 Silver-coated Sub-10 micron Particles

Category Ceramic , Glass , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Potters Industries
Trade Name Conduct-O-Fil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries Conduct-O-Fil® SC04P10 Silver-coated Sub-10 micron Particles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications include conductive inks, conductive adhesives, partial replacement of pure silver powder. Features good conductivity, possible blends/ replacement of 100% pure silver, silver/glass has one third the density of pure silver, narrow particle size distribution.Information provided by Potters Industries.
Physical Properties Metric English Comments
Particle Size 4.0 µm
4.0 µm
Average Diameter
Component Elements Properties Metric English Comments
Silver, Ag 10 %
10 %
by weight
Descriptive Properties Value Comments
Core Material Copper