Polyram RamTough RZ220 Polycarbonate, Injection Molding

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamTough RZ220 Polycarbonate, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 60.0 MPa
>= 8700 psi
ASTM-D638
Elongation at Break >= 75 %
>= 75 %
ASTM-D638
Flexural Strength >= 90.0 MPa
>= 13100 psi
ASTM D790
Flexural Modulus >= 2.20 GPa
>= 319 ksi
ASTM-D790
Izod Impact, Notched 7.00 J/cm - NB

@Temperature 23.0 °C
13.1 ft-lb/in - NB

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 130 °C
>= 266 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) >= 120 °C
>= 248 °F
DIN 53461
Vicat Softening Point 145 °C
293 °F
ASTM-D1525
Flammability, UL94 V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in