Polyram RamTough PZ726 Polycarbonate, Impact Modified, UV Stabilized

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Impact Modified
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamTough PZ726 Polycarbonate, Impact Modified, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An impact modified, UV stabilized polycarbonate for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 2577
Melt Flow 17 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ISO 527
Elongation at Break 120 %
120 %
ISO 527
Flexural Strength 98.0 MPa
14200 psi
ISO 178
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 94.0 kJ/m²
44.7 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ISO 75
Vicat Softening Point 148 °C
298 °F
ISO 306
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Glow Wire Test 825 °C
1520 °F
G.W.I.T; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093