Polyram RamTough PZ506 Polycarbonate, UV Stabilized, Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamTough PZ506 Polycarbonate, UV Stabilized, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV stabilized, flame retardant polycarbonate for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption at Saturation 0.12 %
0.12 %
ISO 62
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 2577
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ISO 527
Elongation at Break 100 %
100 %
ISO 527
Tensile Modulus 2.00 GPa
290 ksi
ISO 527
Flexural Strength 105 MPa
15200 psi
ISO 178
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
ISO 75
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Dielectric Constant 3.2

@Frequency 1.00e+6 Hz
3.2

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60250