Polyram RamTough PZ320G2 Polycarbonate, 10% Glass Fiber, Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamTough PZ320G2 Polycarbonate, 10% Glass Fiber, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% glass fiber reinforced, flame retardant polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
DIN 53479
Water Absorption 0.12 %
0.12 %
DIN 53495
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM-D638
Elongation at Break 15 %
15 %
ASTM-D638
Tensile Modulus 3.10 GPa
450 ksi
ASTM-D790
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM-D790
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0