Material Notes:
40% Carbon fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
DIN 53479
Water Absorption 0.070 %
0.070 %
DIN 53495
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
Melt Flow 5.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 135 MPa
19600 psi
ASTM-D638
Elongation at Break 1.5 %
1.5 %
ASTM-D638
Tensile Modulus 19.5 GPa
2830 ksi
ASTM-D790
Flexural Strength 185 MPa
26800 psi
ASTM D790
Flexural Modulus 13.5 GPa
1960 ksi
ASTM-D790
Izod Impact, Notched 0.550 J/cm

@Temperature 23.0 °C
1.03 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Electrical Properties Metric English Comments
Dielectric Strength 30.0 kV/mm
762 kV/in
VDE 0303/4