Material Notes:
30% Glass-fiber reinforced, heat stabilized PET for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
DIN 53479
Water Absorption 0.50 %
0.50 %
DIN 53495
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 135 MPa
19600 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
ASTM-D790
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 224 °C
435 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
VDE 0303/4