Material Notes:
13% glass fiber reinforced SAN for low warpage and high rigidity injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479
Water Absorption 0.10 %
0.10 %
DIN 53495
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM-D638
Elongation at Break 2.5 %
2.5 %
ASTM-D638
Flexural Strength 140 MPa
20300 psi
ASTM-D790
Flexural Modulus 5.00 GPa
725 ksi
ASTM-D790
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53482