Polyram RamShine PVS701 AES, UV Stabilized

Category Polymer , Thermoplastic , AES Polymer , AES, Extruded
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamShine PVS701 AES, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV stabilized injection molding AESInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Melt Flow 11 g/10 min

@Load 2.10 kg,
Temperature 220 °C
11 g/10 min

@Load 4.63 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM-D785
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM-D638
Elongation at Break 12 %
12 %
ASTM-D638
Tensile Modulus 2.40 GPa
348 ksi
ASTM-D790
Flexural Strength 70.0 MPa
10200 psi
ASTM-D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM-D790
Izod Impact, Notched 2.40 J/cm

@Temperature 23.0 °C
4.50 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Hot Ball Pressure Test 90.0 °C
194 °F
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C
192 °F
DIN 53461