Polyram RamShine PV201 ABS, High Flow

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamShine PV201 ABS, High Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High flow ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Melt Flow 25 g/10 min

@Load 10.0 kg,
Temperature 220 °C
25 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM-D785
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM-D638
Elongation at Break 35 %
35 %
ASTM-D638
Flexural Strength 90.0 MPa
13100 psi
ASTM-D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM-D790
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
DIN 53461
Vicat Softening Point 100 °C
212 °F
ASTM-D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in