UV stabilized polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
DIN 53479
Water Absorption >= 0.030 %
>= 0.030 %
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
0.012 - 0.025 in/in
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM-D785
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM-D638
Elongation at Break 25 %
25 %
ASTM-D638
Flexural Modulus 1.35 GPa
196 ksi
ASTM-D790
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
DIN 53461
Vicat Softening Point 150 °C
302 °F
ASTM-D1525
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
DIN 53482
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53482
Dielectric Constant 2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
VDE 0303/4