Material Notes:
40% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM-D785
Tensile Strength, Yield 95.0 MPa
13800 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 140 MPa
20300 psi
ASTM D790
Flexural Modulus 6.50 GPa
943 ksi
ASTM-D790
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
140 °C
284 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 153 °C
307 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in