Material Notes:
polypropylene with molybdenum for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
DIN 53479
Linear Mold Shrinkage 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM-D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM-D638
Elongation at Break 80 %
80 %
ASTM-D638
Flexural Strength 45.0 MPa
6530 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM-D790
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Users viewing this material also viewed the following: