Material Notes:
30% mineral and glass fiber reinforced, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM-D638
Elongation at Break 5.0 %
5.0 %
ASTM-D638
Tensile Modulus 5.20 GPa
754 ksi
ASTM-D790
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 3.60 GPa
522 ksi
ASTM-D790
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in