Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamOfin PPC342M6 Polypropylene, 30% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPC342M6 Polypropylene, 30% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% mineral filled, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM-D638
Elongation at Break 35 %
35 %
ASTM-D638
Tensile Modulus 4.20 GPa
609 ksi
ASTM-D790
Flexural Strength 45.0 MPa
6530 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM-D790
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
120 °C
248 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C
138 °F
DIN 53461
Vicat Softening Point 140 °C
284 °F
ASTM-D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Users viewing this material also viewed the following: