Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamLloy PZF101 PC/PBT Alloy, Chemical Resistance

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamLloy PZF101 PC/PBT Alloy, Chemical Resistance.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC/PBT alloy for injection molding applications, low temperature and chemical resistance.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage 0.000030 cm/cm
0.000030 in/in
ISO 2577
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 250 °C
18 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527
Elongation at Break 135 %
135 %
ISO 527
Tensile Modulus 1.80 GPa
261 ksi
ISO 527
Flexural Strength 75.0 MPa
10900 psi
ISO 178
Flexural Modulus 1.70 GPa
247 ksi
ISO 178
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
ISO 180
65.0 kJ/m²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75
Flame Spread 10 mm/min
0.39 in/min
FMVSS302
Users viewing this material also viewed the following: