Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamLloy PFS302G14 ASA/PBT Alloy, 14% Glass Fiber

Category Polymer , Thermoplastic , ASA Polymer , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + ASA Blend, Glass Fiber Reinforced
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamLloy PFS302G14 ASA/PBT Alloy, 14% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
14% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ISO 2577
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 275 °C
15 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 4.80 GPa
696 ksi
ISO 527
Flexural Strength 190 MPa
27600 psi
ISO 178
Flexural Modulus 4.10 GPa
595 ksi
ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
401 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250